STAVITRODE A 22 has a rutile coating and an alloyed core, and it can be welded on AC. Joining corrosion-proof, highly heat-proof & non-scaling CrNi-steels that see service temperatures upto 1200°C is its main role. Cr-, CrSi-, and CrAl steels can be joint welded with it, and low alloy base metals can be clad. The weld metal alloy is highly hot-crack-proof & chemical corrosion resistant.

Keep the temperature as low as possible while welding. On ferritic base materials, annealing to 250°C and then post-weld tempering to 700°C is a requirement.

A good choice when stainless of unknown grade must be joined to itself or to carbon steels.

Common uses include furnace-construction, kiln anchor joining, canthol wire joining, valves, heat exchangers, fittings and pipelines.

ميزات فريدة:

  • High alloy content lets it serve at high temperature, with scale resistance up to 1200°C.
  • Spatter emission is extra low, which minimizes clean-up, and arc transfer is extremely smooth, with no turbulence.
  • The weld metal is non-magnetic.
  • Short arc length and ultra low heat.
  • Structure is fully austenitic.
  • Highly resistant to hot-cracking & chemical corrosion.

تفاصيل المنتج

المواصفات الرئيسية:

Mechanical Properties of Weld Metal (Typical)
Alloy Base قوة الخضوع
N/mm2(min)
قوة الشد
N/mm2(min)
Elongation
A5(%)(min)
Impact
(J) (min)
Cr, Ni, Mo 410 580 37 70 J at 0°C

دعنا نجد لك الحل الأمثل في مجال اللحام.

شاركنا متطلباتك. سنساعدك في اتخاذ الخطوة التالية.

Security code image

تُستخدم بياناتك فقط للرد على استفسارك. سياسة الخصوصية

هل تفضل الاتصال؟ +91-9319198528 (Domestic) +91 74287 49656 (International)

اتصل بستانفاك

استفسار سريع

أخبرنا بما تحتاجه. سيتواصل معك فريقنا.

Security code image

بإرسالك هذا الطلب، فإنك توافق على أن يتم التواصل معك بشأن استفسارك. سياسة الخصوصية.