Industries · Sugar

Welding solutions for every stage of the sugar mill

A sugar mill runs on a short season and cannot stop for a rebuild. Cane fibre and grit wear the knives, the fibrizer and the roller surfaces; hot acidic juice eats condensers and pump bodies; cast trash beams crack under shock. Pick an area of the mill to see which components fail, how they fail, and the STANVAC range that puts them back to work.

23
Components mapped
5
Mill areas
500+
Authorised distributors
Isometric view of a sugar mill — a walled cane yard with a grab crane over stacked cane and loaded carts, a long milling tandem under its shed, a tall evaporator and pan block with its chimney, a bagasse-fired boiler and turbo-alternator hall with the workshop beside it, the centrifugal station and bagged sugar store, and a cooling pond in the middle of the roads.
Sugar mill site 23 components mapped Click a numbered pin on the mill
Mill area

All mill areas

Every mapped component across the sugar mill.

Component Base metal Wear factor Mill area Recommended solution
Cane Loading Spikes Carbon Steel Wear Cane Yard & Preparation Nátery a nanášanie matríc (opens in a new tab)
Cane Grabs Carbon Steel Wear Cane Yard & Preparation Nátery a nanášanie matríc (opens in a new tab)
Cane Leveller Arms Carbon Steel Wear Cane Yard & Preparation Nátery a nanášanie matríc (opens in a new tab)
Cane Cutting Knives Carbon Steel Wear Cane Yard & Preparation STAVITRODE A 74 (opens in a new tab) Elektródy s tvrdým povrchom
Fibrizer Carbon Steel Wear Cane Yard & Preparation STAVITRODE A 75 (opens in a new tab) Elektródy s tvrdým povrchom
Striking Bar Of Anvil Oceľ Wear Milling Tandem STAVITRODE A 25 (opens in a new tab) Elektródy na nanášanie plášťov a matríc
Tail Bar Low Alloy Steel Wear Milling Tandem STAVITRODE A 25 (opens in a new tab) Elektródy na nanášanie plášťov a matríc
Trash Plate Carbon Steel Teeth Wear Milling Tandem STAVITRODE A 75 (opens in a new tab) Elektródy s tvrdým povrchom
Scraper Plate Carbon Steel Teeth Wear Milling Tandem STAVITRODE A 75 (opens in a new tab) Elektródy s tvrdým povrchom
Trash Beam Cast Iron Crack Milling Tandem Liatinové elektródy (opens in a new tab)
Crusher Roller Steel / Cast Iron Wear Slip Milling Tandem STAVITRODE A 80(S) (opens in a new tab) Elektródy s tvrdým povrchom
Roller Pinion Carbon Steel Wear Milling Tandem STAVITRODE A 11 (opens in a new tab) Oprava - Spájanie elektródy
Square Coupling Steel / Cast Iron Wear Milling Tandem STAVITRODE A 56 (opens in a new tab) Oprava - Spájanie elektródy
Juice Ring Oceľ Wear Milling Tandem STAVITRODE A 84 (opens in a new tab) Elektródy na nanášanie plášťov a matríc
SS Condenser SS 316 Wear / Fabrication Boiling House Stainless steel electrodes (opens in a new tab)
Juice Pump Cast Iron Wear Boiling House STAVITRODE A 42 (opens in a new tab) Elektródy na zváranie liatiny
Magma Pump Bronze Wear Boiling House Not available
Brake Drum Cast Iron Wear Boiling House STAVITRODE A 42 (opens in a new tab) Elektródy na zváranie liatiny
Centrifuge Shaft Alloy Steel Wear Centrifugals & Drives STAVITRODE A 24 (opens in a new tab) Oprava - Spájanie elektródy
Sprocket Oceľ Wear Centrifugals & Drives STAVITRODE A 71 (opens in a new tab) Elektródy s tvrdým povrchom
Pump Shaft Keys Oceľ Wear Centrifugals & Drives STAVITRODE A 24 (opens in a new tab) Oprava - Spájanie elektródy
Turbine Casing Oceľ Crack Power House & Workshop STAVITRODE A 24 (opens in a new tab) Oprava - Spájanie elektródy
Unknown Metal Oceľ Wear/Crack Power House & Workshop STAVITRODE A 24 (opens in a new tab) Oprava - Spájanie elektródy

Magma Pump

Boiling House
Base metal Bronze
Wear factor Wear
Not available
Showing 23 of 23 components Confirm the grade with our application engineers before welding
How sugar mill components fail
  1. Abrasion

    Cane fibre, grit and field mud cutting into knives, fibrizer tips and roller surfaces.

  2. Grooving & slip

    Roller and trash-plate teeth rounding off until the mill stops gripping and extraction falls.

  3. Corrosion

    Hot acidic juice and vapour eating condensers, juice pumps and the pan-floor pipework.

  4. Cracking

    Cast trash beams, housings and turbine casings split by shock loading or an overtightened mill.

Send us the component.
We’ll send the procedure.

Base metal, wear factor and a photograph — an application engineer comes back with the consumable, the parameters and the expected life gain.